Metastable alumina formation during oxidation of FeCrAl and its suppression by surface treatmentsE. N'Dah; A. Galerie; Y. Wouters; D. Goossens; D. Naumenko; V. Kochubey; W. J. Quadakkers20052005, vol.56, no.12
Effects of minor additions and impurities on oxidation behaviour of FeCrAl alloys. Development of novel surface coatings compositionsV. Kochubey; H. Al-Badairy; G. Tatlock; J. Le-Coze; D. Naumenko; W. J. Quadakkers20052005, vol.56, no.12
Lifetime extension of FeCrAlRE alloys in air: Potential roles of an enhanced Al-reservoir and surface pre-treatmentM. J. Bennett; J. R. Nicholls; N. J. Simms; D. Naumenko; W. J. Quadakkers; V. Kochubey; R. Fordham; R. Bachorczyk; D. Goossens; H. Hattendorf; A. B. Smith; D. Britton20052005, vol.56, no.12
The effect of gas composition and contaminants on the lifetime of surface-treated FeCrAlRE alloysG. J. Tatlock; H. Al-Badairy; R. Bachorczyk-Nagy; R. Fordham20052005, vol.56, no.12
Development of novel diffusion coatings for 9-12% Cr ferritic-martensitic steelsV. Rohr; M. Schutze; E. Fortuna; D. N. Tsipas; A. Milewska; F. J. Perez20052005, vol.56, no.12
Gaseous corrosion of alloys and novel coatings in simulated environments for coal, waste and biomass boilersJ. Kalivodova; D. Baxter; M. Schutze; V. Rohr20052005, vol.56, no.12
Steam oxidation and its potential effects on creep strength of power station materialsL. Nieto Hierro; V. Rohr; P. J. Ennis; M. Schutze; W. J. Quadakkers20052005, vol.56, no.12
The erosion-corrosion resistance of uncoated and aluminized 12% chromium ferritic steels under fluidized-bed conditions at elevated temperatureE. Huttunen-Saarivirta; S. Kalidakis; F. H. Stott; V. Rohr; M. Schutze20052005, vol.56, no.12
New oxidation-resistant coatings for steam power plants at 650℃M. Scheefer; R. Knodler; B. Scarlin; A. A. Bruna; D. N. Tsipas20052005, vol.56, no.12
Silicon surface treatment via CVD of inner steel tube surfacesK. Berreth; K. Maile; A. Lyutovich20052005, vol.56, no.12